Product - ESD FABRIC
ESD TRICOT FABRIC
CONDUCTIVE TRICOT FABRIC
Technical Specification | Unit | Conditions | Method | |
Material | PET 90%, Carbon 10% | |||
Type of weave | Knitted-4Bar | |||
Weight | 160 | g/sqm | ||
Finish | piece Dyed | |||
Density:warp x fill | 31 x 37 | threads/inch | KS K 0512 | |
Tensile Strength: Warp Fill | 40.1 | Kg | Grab Method, Cre Type | KS K 0520 |
57 | ||||
PILLING | 5 | class | ICI Box Method/4hrs | KS K 0503 |
Abrasion | Over 20,000 | Cycles | Martindale Method | KS K 0604 |
Dimensional Charge | Warpwise:2.0 | % | after 1 Wash (30 °C, Flat dry) | KS K 0465 |
Fillingwise:1.0 | ||||
Test Results | unit | conditions | Method | |
Air Permeability cm²/cm³/sec. | 124 | Test area:38cm² | KS K 0570 | |
Test pressure:125pa | (Frazier Method) | |||
Water Vapour Transmission g/m².hour | 329 | Cacl2 Method | KS K 0594 | |
40 ±2°C/ RH 90±2% | ||||
Pore Size | 153.7 | µm | BS 3321 | |
Static Decay(Decay half life) | 1.3 | sec | ASTM D 4238 | |
Surface Resistivity | Below 1.5 x 10(6) | º | 20°C,65%RH | AATCC 76 |
100V | ||||
Electrostatic Propensity | Below 10 | Volt | 20±2°c, 65±2%RH, 400rpm | KS K 0555-1983 |
Cotton Fabric | B Method |